Thanks again to Brian for putting me on the right path. Started with the die made from Plexiglas in the containment vessel.
Put the vessel in the press.
Pumped it up to 5500 and removed from press.
Removed the metal from the vessel and trimmed.
Soldered on the back and trimmed.
I found that if I used a little lube on the metal things went better especially with thinner metal. Any corrections suggestions or comments welcome.